| Test | Specification | Typical | Method | Source |
|---|---|---|---|---|
| Assay (n-amyl acetate) | ≥99% | 99.6 % | — | Supplier specification |
| Acidity (as acetic acid) | 0.030 % max | 0.005 % | ASTM D1613 / titration | Interpreted |
| Water | 0.10 % max | 0.03 % | ASTM E1064 / Karl Fischer | Interpreted |
Specification values are guaranteed limits. Typical values are representative of production lots and are not guaranteed. Lot-specific certificates of analysis ship with every order.
| Property | Value | Source |
|---|---|---|
| Appearance | Liquid | Supplier specification |
| Form | Liquid | Published reference |
| Odor | Pear-like odor | Published reference |
| Specific Gravity (20 °C) | 0.873 - 0.879 | Interpreted |
| Density | 0.876 at 59 °F (USCG, 1999) - Less dense than water; will float | Published reference |
| Boiling Point | 145 - 152 C | Interpreted |
| Melting Point | -109.3 °F (NTP, 1992) | Published reference |
| Flash Point | 77 °F (NTP, 1992) | Published reference |
| Vapor Pressure | 4 mmHg at 68 °F ; 5 mmHg at 74.7 °F; 760 mmHg at 288 °F (NTP, 1992) | Published reference |
| Solubility (water) | less than 1 mg/mL at 66 °F (NTP, 1992) | Published reference |
Polar solvent — purity vs. intended end-use (electronics, pharma, general industrial) is the dominant grade consideration. See application guidance for grade selection.
| Material | Rating | Max T (°C) | Notes | Source |
|---|---|---|---|---|
Buna-N (NBR) elastomer | Fair | 60 | Acceptable for alcohols; poor for ketones. | Parker O-ring Chemical Compatibility |
EPDM elastomer | Fair | — | Good for alcohols, poor for esters | Cole-Parmer Chemical Compatibility |
Viton (FKM) elastomer | Fair | 80 | Swells in acetone and esters; avoid for those. | Parker O-ring Chemical Compatibility |
FFKM (Kalrez) fluoropolymer | Excellent | 200 | Premium ester / ketone sealing | Cole-Parmer Chemical Compatibility |
PTFE fluoropolymer | Excellent | 200 | Universal solvent compatibility. | Cole-Parmer Chemical Compatibility |
Borosilicate Glass glass ceramic | Excellent | 100 | Universally inert. | Cole-Parmer Chemical Compatibility |
Glass (borosilicate) glass ceramic | Excellent | 100 | Inert | Cole-Parmer Chemical Compatibility |
316L Stainless Steel metal | Excellent | 80 | Inert; preferred for high-purity solvent service. | Cole-Parmer Chemical Compatibility |
Aluminium metal | Good | 40 | Acceptable; avoid prolonged wet contact | Cole-Parmer Chemical Compatibility |
Carbon Steel metal | Fair | 50 | Trace moisture causes rust; flash-rust prevention required. | Cole-Parmer Chemical Compatibility |
HDPE thermoplastic | Fair | 40 | Swells with many polar solvents; verify per solvent. | Cole-Parmer Chemical Compatibility |
PP thermoplastic | Good | 50 | Acceptable but watch swelling with esters | Cole-Parmer Chemical Compatibility |
PVC thermoplastic | Fair | 25 | Esters soften PVC; avoid for esters | Cole-Parmer Chemical Compatibility |
Ratings reflect the service envelope (concentration × temperature) shown. Always confirm against your specific duty cycle and contact-time before equipment selection. The most cautious rating across overlapping references is shown.
Showing 13 of 13 materials compatible at the selected envelope.
| Material | Rating | Max T (°C) | Notes |
|---|---|---|---|
Buna-N (NBR) elastomer | Fair | 60 | Acceptable for alcohols; poor for ketones. |
EPDM elastomer | Fair | — | Good for alcohols, poor for esters |
Viton (FKM) elastomer | Fair | 80 | Swells in acetone and esters; avoid for those. |
FFKM (Kalrez) fluoropolymer | Excellent | 200 | Premium ester / ketone sealing |
PTFE fluoropolymer | Excellent | 200 | Universal solvent compatibility. |
Borosilicate Glass glass ceramic | Excellent | 100 | Universally inert. |
Glass (borosilicate) glass ceramic | Excellent | 100 | Inert |
316L Stainless Steel metal | Excellent | 80 | Inert; preferred for high-purity solvent service. |
Aluminium metal | Good | 40 | Acceptable; avoid prolonged wet contact |
Carbon Steel metal | Fair | 50 | Trace moisture causes rust; flash-rust prevention required. |
HDPE thermoplastic | Fair | 40 | Swells with many polar solvents; verify per solvent. |
PP thermoplastic | Good | 50 | Acceptable but watch swelling with esters |
PVC thermoplastic | Fair | 25 | Esters soften PVC; avoid for esters |
Transport descriptions reflect 49 CFR 172.101 lookup at time of publication. Sourced data: ECHA CLP Annex VI for harmonised classifications, NIOSH Pocket Guide for REL/IDLH, OSHA Z-Tables for PEL. Always verify against the latest regulatory text before shipment-critical decisions.
One zipped download containing the TDS, SDS, latest lot COA (when available), and a fresh Letter of Continuing Guaranty for Amyl Acetate. Every file included is SHA-256 hashed and listed in a manifest your QA team can audit.
Applications are drawn from published manufacturer and supplier documentation; each is sourced. Suitability for a specific use is the buyer's to confirm.
For full hazard, PPE, and emergency response guidance, refer to the Safety Data Sheet (SDS) for this product. The SDS controls in all cases where guidance differs.
UN1104, Amyl acetates, 3, PG III
Sourced from 49 CFR 172.101. Confirm against shipping documents and carrier requirements before tender.
Last reviewed 2026-07-17 by Andre Taki, DOT Hazmat Specialist.
| Version | Date | Change | Trigger |
|---|---|---|---|
| 1.3 | 2026-08-05 | Canonical data updated: 1 field changed via the provenance/adjudication pipeline.
| canonical_change |
| 1.2 | 2026-07-22 | Canonical data updated: 1 field changed via the provenance/adjudication pipeline.
| canonical_change |
| 1.1 | 2026-07-17 | Canonical data re-verified: 7 fields updated against independent vendor SDSs, CLP Annex VI, 49 CFR, and OSHA HazCom 2024 (GHS classification, hazard/precautionary codes, signal word, physical properties as applicable).
| canonical_change |
| 1.0 | 2026-05-20 | Initial URL-first TDS published from canonical chemistry registry. | initial |
This Technical Data Sheet is provided for technical reference. The Safety Data Sheet (SDS) controls in all cases where guidance differs. Values reflect Alliance Chemical canonical data at time of generation; subsequent revisions are recorded in the Revision History above.