| Material | Calificación | T máx (°C) | Notas | Fuente |
|---|---|---|---|---|
Buna-N (NBR) elastomer | Aceptable | 60 | Acceptable for alcohols; poor for ketones. | Parker O-ring Chemical Compatibility |
EPDM elastomer | Aceptable | — | Good for alcohols, poor for esters | Cole-Parmer Chemical Compatibility |
Viton (FKM) elastomer | Aceptable | 80 | Swells in acetone and esters; avoid for those. | Parker O-ring Chemical Compatibility |
FFKM (Kalrez) fluoropolymer | Excelente | 200 | Premium ester / ketone sealing | Cole-Parmer Chemical Compatibility |
PTFE fluoropolymer | Excelente | 200 | Preferred for all polar solvents | Cole-Parmer Chemical Compatibility |
Borosilicate Glass glass ceramic | Excelente | 100 | Universally inert. | Cole-Parmer Chemical Compatibility |
Glass (borosilicate) glass ceramic | Excelente | 100 | Inert | Cole-Parmer Chemical Compatibility |
316 stainless steel metal | Excelente | 60 | Standard alcohol / ester service | Cole-Parmer Chemical Compatibility |
316L Stainless Steel metal | Excelente | 80 | Inert; preferred for high-purity solvent service. | Cole-Parmer Chemical Compatibility |
Aluminium metal | Bueno | 40 | Acceptable; avoid prolonged wet contact | Cole-Parmer Chemical Compatibility |
Carbon steel metal | Bueno | 40 | Acceptable for short-term storage | Cole-Parmer Chemical Compatibility |
Carbon Steel metal | Aceptable | 50 | Trace moisture causes rust; flash-rust prevention required. | Cole-Parmer Chemical Compatibility |
HDPE thermoplastic | Aceptable | 40 | Swells with many polar solvents; verify per solvent. | Cole-Parmer Chemical Compatibility |
PP thermoplastic | Bueno | 50 | Acceptable but watch swelling with esters | Cole-Parmer Chemical Compatibility |
PVC thermoplastic | Aceptable | 25 | Esters soften PVC; avoid for esters | Cole-Parmer Chemical Compatibility |
Las calificaciones reflejan la envolvente de servicio (concentración × temperatura) indicada. Confirme siempre con su ciclo de trabajo y tiempo de contacto específicos antes de seleccionar el equipo. Se muestra la calificación más cautelosa entre las referencias que se solapan.
Mostrando 15 de 15 materiales compatibles en la envolvente seleccionada.
| Material | Calificación | T máx (°C) | Notas |
|---|---|---|---|
Buna-N (NBR) elastomer | Aceptable | 60 | Acceptable for alcohols; poor for ketones. |
EPDM elastomer | Aceptable | — | Good for alcohols, poor for esters |
Viton (FKM) elastomer | Aceptable | 80 | Swells in acetone and esters; avoid for those. |
FFKM (Kalrez) fluoropolymer | Excelente | 200 | Premium ester / ketone sealing |
PTFE fluoropolymer | Excelente | 200 | Preferred for all polar solvents |
Borosilicate Glass glass ceramic | Excelente | 100 | Universally inert. |
Glass (borosilicate) glass ceramic | Excelente | 100 | Inert |
316 stainless steel metal | Excelente | 60 | Standard alcohol / ester service |
316L Stainless Steel metal | Excelente | 80 | Inert; preferred for high-purity solvent service. |
Aluminium metal | Bueno | 40 | Acceptable; avoid prolonged wet contact |
Carbon steel metal | Bueno | 40 | Acceptable for short-term storage |
Carbon Steel metal | Aceptable | 50 | Trace moisture causes rust; flash-rust prevention required. |
HDPE thermoplastic | Aceptable | 40 | Swells with many polar solvents; verify per solvent. |
PP thermoplastic | Bueno | 50 | Acceptable but watch swelling with esters |
PVC thermoplastic | Aceptable | 25 | Esters soften PVC; avoid for esters |
Las descripciones de transporte reflejan la consulta del 49 CFR 172.101 en el momento de la publicación. Datos de origen: anexo VI del Reglamento CLP de la ECHA para las clasificaciones armonizadas, NIOSH Pocket Guide para REL/IDLH, tablas Z de la OSHA para PEL. Verifique siempre con el texto reglamentario más reciente antes de tomar decisiones críticas para el envío.
Una única descarga comprimida que contiene la FTP, la FDS, el CdA del último lote (cuando esté disponible) y una Carta de Garantía Continua reciente para Propylene Glycol Inhibited ACS Grade. Cada archivo incluido lleva un hash SHA-256 y figura en un manifiesto que su equipo de CC puede auditar.
Propylene Glycol Inhibited ACS Grade (ACS Grade) es un disolvente polar. La selección del grado (técnico, ACS, electrónico, USP) determina los niveles aceptables de residuos e impurezas para el uso final previsto.
Inflamable. Conecte equipotencialmente y a tierra el equipo durante el trasvase. Verifique que el grado coincida con la especificación de uso final antes de sustituirlo.
Para obtener orientación completa sobre peligros, EPP y respuesta a emergencias, consulte la ficha de datos de seguridad (FDS) de este producto. La FDS prevalece en todos los casos en que la orientación difiera.
Última revisión el 2026-05-20 por Hossein Taki, Vice President (Vice President, Alliance Chemical · CAGE Code 1LT50 · DOT Hazmat Registrant #2188383).
| Versión | Fecha | Cambio | Desencadenante |
|---|---|---|---|
| 1.0 | 2026-05-20 | Initial URL-first TDS published from canonical chemistry registry. | initial |
Esta hoja de datos técnicos se proporciona como referencia técnica. La ficha de datos de seguridad (FDS) prevalece en todos los casos en que la orientación difiera. Los valores reflejan los datos canónicos de Alliance Chemical en el momento de la generación; las revisiones posteriores se registran en el historial de revisiones anterior.